# PCB Glossary: Thermal cycling

**URL:** <https://sierraconnect.protoexpress.com/t/pcb-glossary-thermal-cycling/4438>\
**Category:** PCB Glossaries\
**Created:** [September 3, 2026, 11:04am UTC](https://sierraconnect.protoexpress.com/t/pcb-glossary-thermal-cycling/4438 "2026-09-03T11:04:54Z")\
**Posts on this page:** 1\
**Page:** 1

<div class="post-metadata">

**Author:** ![Mohamed\_Faheemuddin](https://avatars.discourse-cdn.com/v4/letter/m/4da419/32.png) [@Mohamed\_Faheemuddin](https://sierraconnect.protoexpress.com/u/Mohamed_Faheemuddin)\
**Post date:** [September 3, 2026, 11:04am UTC](https://sierraconnect.protoexpress.com/t/pcb-glossary-thermal-cycling/4438/1 "2026-09-03T11:04:54Z")

</div>

PCB thermal cycling is a type of circuit board test that exposes a board to repeated predetermined high and low temperatures. It evaluates how well the circuit board materials, interconnections, and components withstand thermal stress.

Understanding thermal cycling during layout, stack-up design, and component selection helps you prevent potential defects such as PTH barrel cracking, inner-layer separation, delamination, and solder fatigue caused by thermal shock from improper [thermal profiling during PCB assembly](https://www.protoexpress.com/blog/thermal-profiling-pcb-assembly-unsung-hero/?utm_source=sierraconnect&utm_medium=display&utm_campaign=glossary%2Bpcb%2Bthermal%2Bcycling%2Bsep%2B2026).

Factors such as differences in material expansion, board thickness, via construction, copper features, and solder joint design can influence how a PCB responds to repeated temperature changes.

 ![PCB thermal cycling testing showing cyclic exposure to high and low temperatures](https://global.discourse-cdn.com/sierraconnect/original/1X/1dab82215427ef536be6c6f40e8e5dee8b8357cd.jpeg)

**Quick design tips for better thermal cycling performance**

- Choose laminates with a low Z-axis CTE (\<70 ppm/°C) to limit expansion through the board thickness and reduce stress on PTHs and vias during thermal cycling.
- Avoid placing large BGAs or heavy components near board edges to reduce the stress on solder joints during thermal cycling.
- Maintain balanced copper distribution across layers to reduce uneven heating and warpage.
- Verify that the selected laminate’s Tg is comfortably above the product’s expected operating temperature range.
- Place test coupons on the fabrication panel to validate the board’s integrity under standard thermal cycling profiles (for example, IPC-TM-650 2.6.7)